have higher Tg. And, its blends with PES and PPS are extremely compatible. Full Article of PEEK Restriction of PEEK Expensive, suitable for highly demanding application Processing at high temperature levels Attached by some acids, such as conc. Sulphuric, Nitric, Chromic and is assaulted by halogens and sodium Low resistance to UV light How PEEK is Made? How PEEK is Manufactured? PEEK polymers are gotten by step-growth polymerization by the dialkylation of bisphenolate salts.
The polymer is then separated by elimination of alkali metal fluoride and the polymerization solvent. Because of its fairly stiff fragrant polymer backbone, the polymer displays a few of the highest thermal transitions among numerous other business polymers and hence can be used at temperatures as high as 240C. Processing Conditions for PEEK Polymers Processing Issues for PEEK Polymers PEEK can be processed by traditional techniques such as injection molding, extrusion, compression molding etc.
As a direct thermoplastic, Polyetheretherketone can be melt processed in the temperature level variety of 370 to 420C. While processing Polyetheretherketone, no destructive gases are evolved. Prior to processing Polyetheretherketone, drying is advised for 3 hours at 150C or 2 hours at 180C. This is done to avoid any molding defects. Polyetheretherketone can be processed by injection molding and extrusion.
Post condensation at 200C is possible but it is not recommended for applications needing high dimensional stability. PEEK appropriates for injection of extremely small parts with tight dimensional tolerances. Injection pressure: 70-140 Mpa Mold shrinkage: Unfilled 1. 2-2. 4%, Filled 0. 1-1. 1% Extrusion Cooling temperature have a strong influence on crystallinity and after that on efficiencies.
Cooling cylinders at 170C result in nontransparent and extremely crystalline product. It is also possible to produce focused or bioriented films by the procedure of extrusion. 3D printing Thanks to its unique residential or commercial properties, of PEEK permits building of almost any complicated design geometry, which can not be made utilizing other innovations.
Nozzle temperature: 360-400 degrees Celsius Heated bed: 120 degrees Celsius It is an outstanding prospect for FFF due to its low wetness absorption instead of other typical FFF products, such as Acrylonitrile Butadiene Styrene (ABS). Find Suitable Polyetheretherketone (PEEK) Grade View a wide variety of polyetheretherketone (PEEK) grades available in the market today, examine technical information of each item, get technical support or demand samples.